Funct. Mater. 2026; 33 (3): 537-543.
The oxoacidic properties and deoxidization features of LiCl-based melts at 973 K
1Institute for Scintillation Materials, National Academy of Sciences of Ukraine, Nauky avenue, 60, 61001, Kharkiv, Ukraine
2V.N.В Karazin Kharkiv National University, Svobody Sq., 4, 61022, Kharkiv, Ukraine
3Poltava V.G. Korolenko National Pedagogical University, Ostrogradsky str., 2, Poltava, Ukraine
The oxoacidic properties of LiCl melt were investigated on the basis potentiometric determination of magnesium oxide solubility at 973 K using the Pt(O2)ZrO2(Y2O3) indicator electrode. The solubility product of MgO pKs, MgO, LiCl was estimated as 4.57 in the molality scale(pKsx, MgO, LiCl = 7.33 in molar fractions), i.e. magnesium oxide is slightly soluble in the LiCl melt. The oxobasicity index of the LiCl melt is 4.29, i.e., it has stronger oxoacidic properties than the melt of the eutectic KCl-LiCl mixture (3.50), which is caused by the higher content of lithium cations in pure LiCl melt. The deoxidization of LiCl melt by carbochlorination at 973 K lasts 60 minutes and is limited by residual O2– concentration of 1.9·10–7 mol·kg–1. The chemical reaction of second kinetic order becomes the limiting stage 30 minutes after the process starts and is defined by the rate constant of 3.3 (±0.2)·105 kg·mol–1·min–1. The strong oxoacidic properties of LiCl allow to quantitatively dissolve Eu2O3 which may prove useful from the viewpoint of scintillation materials science. At 973 K the solubility of Eu2O3 is equal to 0.1 mol·kg–1 (or approximately 3.4 % w/w). At the carbochlorination of LiCl melt containing 0.1 g of Eu2O3 the process of dissolving the Eu oxo-derivatives takes 100 min, and the total duration of the process increases to 4 h.
1. H. Lux. «Sauren» und «basen» im schmeltzfluss: die bestimmung der sauerstoffionen-konzentration, Z. Elektrochem., 45 (4) (1939) 303-309. DOI:10.1002/BBPC.19390450405.
2. J. Guo, A. Merwin, C. J. Benmore, Z.-G. Mei, N. C. Hoyt, M. A. Williamson. Fluid structure of molten LiCl-Li solutions, J. Phys. Chem. B, 123 (47) (2019), 10036-10043. DOI: 10.1021/acs.jpcb.9b07479.
3. A. Burak, J. Chamberlain, M.F. Simpson. Study of entrainment of Li2O in product from direct electrolytic reduction of UO2 in molten LiCl–Li2O. Part 1: post-processing and analysis techniques, J. Nucl. Mater., 59 (2020), 529, 151913. DOI: 10.1016/j.jnucmat.2019.151913.
4. J.-M. Hur, S. M. Jeong, Kyeong Youl Jung. Direct electrochemical reduction of titanium dioxide in molten lithium chloride, J. Ind. Eng. Chem., 18 (1) (2012), 438-442. DOI: 10.1016/j.jiec.2011.11.111.
5. E.-Y. Choi, D. H. Heo. Reduction of zirconium oxide compounds by lithium metal as a reductant in molten LiCl salt, J. Nucl. Mater., 2018, 2018512, DOI: 10.1016/j.jnucmat.2018.10.015.
6. B. H. Park, J. Kim. Thermodynamic Analysis on Oxo-acidity of Actinide Oxides for Electrolytic Reduction in Molten Lithium Chloride Salt, Preprint, DOI: 10.21203/rs.3.rs-7208784/v1.
7. J.M. Hur, S. M. Jeong, H. Lee. Underpotential deposition of Li in a molten LiCl-Li2O electrolyte for the electrochemical reduction of U from uranium oxides, Electrochem. Commun., 12(5) (2010) , 706-709. DOI: 10.1016/j.elecom.2010.03.012.
8. M. A. Gonzalez, C. Leavitt, J. M. Holland, M. F. Simpson. UO2 solubility and chemical interactions in molten LiCl-Li2O, J. Nucl. Mater., 599 (2024), 155220. DOI: 0.1016/j.jnucmat.2024.155220.
9. M. Zabłocka-Malicka, W. Szczepaniak. Electrical conductivity of molten lithium chloride – dysprosium (III) chloride system compared to other alkali metal chloride – dysprosium (III) chloride and lithium chloride – lanthanide (III) chloride systems, J. Mol. Liq., 222 (2016), 818-822. DOI: 10.1016/j.molliq.2016.07.100.
10. M. A. Howe, R. L. Mcgreevy. A neutron-scattering study of the structure of molten lithium chloride, Philosophical Magazine B, 58 (5) (1988), 485-495. DOI: 10.1080/13642818808208460.
11. R. Combes, M.N. Levelut, B. Tremillon. Oxoacidity and its influence in the electrochemical properties in molten mixtures of CeCl3 and equimolar NaCl-KCl at 1000 K, Electrochim. Acta, 23 (12) (1978), 1291-1295. DOI: 10.1016/0013-4686(78)80006-1.
12. V.L. Cherginets, T.P. Rebrova, V.A. Naumenko. Oxoacidity scale in molten ionic chlorides and bromides, Fluid Phase Equilib., 401(2015), 77-81 (DOI: 10.1016/j.fluid.2015.05.025).
13. B.V. Grynyov, M.M. Smyrnov, Scintillation material based on activated lithium iodide crystal, Patent of Ukraine No. 77423, 15.12.2006.
14. V.L. Cherginets, T.P. Rebrova, Yu.N. Datsko, V.F. Goncharenko, N.N. Kosinov, R.P. Yavetsky, V.Yu Pedash, Luminescent properties of CsI single crystals grown from the melt treated by EuI2, Cryst.Res.Technol, 47(6) (2012), 684-688 (DOI:10.1002/crat.201200040).
15. V.L. Cherginets, T.P. Rebrova, T.V. Ponomarenko, A.L. Rebrov, O.I. Yurchenko, Y.I. Dolzhenko. Investigation of course of K2SrCl4 melt deoxidization with CCl4 vapor, Reaction Kinetics, Mechanisms and Catalysis, 120 (1) (2017), 31-38. DOI: 10.1007/s11144-016-1099-1.
16. V.L. Cherginets, E.G. Khailova, O.V. Demirskaya. On the solubilities of metal oxides in ionic melt 2 CsBr-KBr at 700°C, Electrochim.Acta, 41 (3) (1996), 463-467. DOI: 10.1016/j.jct.2014.02.001.
17. V.L. Cherginets, O.V. Demirskaya, T.P. Rebrova. Oxobasicity index as a measure of acidic properties of ionic melts: definition and methods of acidity estimation, Molten salts forum, 7 (2000), P.163-166.
18. V.L. Cherginets, V.A. Naumenko, T.V. Ponomarenko, T.P. Rebrova, Features of the kinetics of carbochlorination of KCl-LiCl melt, Voprosy Khimii i Khim. Technologii, No 2 (2013), 138-141.
19. Y. Castrillejo, M. R. Bermejo, R. Pardo, A. M. Martinez. Use of electrochemical techniques for the study of solubilization processes of cerium–oxide compounds and recovery of the metal from molten chlorides, J. Electroanal. Chem., 522 (2), (2002), 124-140. DOI: 10.1016/S0022-0728(02)00717-9.
20. Y. Castrillejo, M. R. Bermejo, E. Barrado, A.M. Martinez, P.D. Arocas. Solubilization of rare earth oxides in the eutectic LiCl-KCl mixture at 450 °C and in the equimolar CaCl2-NaCl melt at 550 °C, J. Electroanal. Chem., 545 (2003), 141–157. DOI: 10.1016/S0022-0728(03)00092-5.